Ki evalyasyon presyon pou tiyo API 5L Klas B?
Tiyo API 5L Klas B se yon tiyo komen pou transmisyon tiyo lwil oliv ak gaz. Sa a se konnen tou kòm tiyo L245 (gade ISO 3183). Yo te rele pou fòs sede minimòm li nan 245 MPa (35,500 psi).
API 5L Gr.B tiyo asye san pwoblèmyo fabrike soti nanwo -bon jan kalite asye kabòn oswa ba-biye asye alyaj atravè pwosesis desen cho-woule oswa frèt-. Espesifikasyon kle yo enkli:
Konpozisyon chimik:
Kabòn (C) Mwens pase oswa egal a 0.28%
Manganèz (Mn) Mwens pase oswa egal a 1.20%
Pwopriyete mekanik:
Fòs sede Pi gran pase oswa egal a 241 MPa
Fòs rupture: 413-517 MPa
Kontwòl soude:
Kabòn ekivalan (Ceq) tipikman mwens pase oswa egal a 0.43% asire soudabilite
API 5L Klas B Tablo Orè Tiyo
| NB | DN | OD (mm) | Orè tiyo | |||||||||
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| SCH 5 | SCH 10 | SCH 20 |
SCH 30 | SCH 40 | SCH 60 | SCH 80 | SCH 100 | SCH 120 | SCH 160 | |||
| 3/4" | 20 | 26.67 | 1.65 | 2.11 | x | 2.41 | 2.87 | x | 3.91 | x | 4.32 | 5.56 |
| 1" | 25 | 33.40 | 1.65 | 2.77 | x | 2.90 | 3.38 | x | 4.55 | x | 5.08 | 6.35 |
| 1.1/2" | 40 | 48.26 | 1.65 | 2.77 | x | 3.18 | 3.68 | x | 5.08 | x | 5.72 | 7.14 |
| 2" | 50 | 60.32 | 1.65 | 2.77 | x | x | 3.91 | x | 5.54 | x | 6.35 | 8.74 |
| 2.1/2" | 65 | 73.02 | 2.11 | 3.05 | x | x | 5.16 | x | 7.01 | x | 7.62 | 9.53 |
| 3" | 80 | 88.9 | 2.11 | 3.05 | x | x | 5.49 | x | 7.62 | x | 8.89 | 11.13 |
| 4" | 100 | 114.3 | 2.11 | 3.05 | x | x | 6.02 | x | 8.56 | x | 11.10 | 13.49 |
| 5" | 125 | 141.3 | 5.77 | 3.4 | x | x | 6.55 | x | 9.53 | x | 12.70 | 15.88 |
| 6" | 150 | 168.27 | 2.77 | 3.4 | x | x | 7.11 | x | 10.97 | x | 14.27 | 18.26 |
| 8" | 200 | 219.07 | 2.77 | 3.76 | 6.35 | 7.04 | 8.18 | 12.7 | 12.70 | 15.06 | 18.24 | 23.01 |
| 10" | 250 | 273.05 | 3.4 | 4.19 | 6.35 | 7.8 | 9.27 | 12.7 | 15.06 | 18.24 | 21.41 | 28.58 |
| 12" | 300 | 323.85 | 4.19 | 4.57 | 6.35 | 8.38 | 10.31 | 12.7 | 17.45 | 21.41 | 25.40 | 33.32 |
tès ak enspeksyon
Devyasyon dimansyon
bon jan kalite sifas yo
analiz konpozisyon chimik
tès pwopriyete mekanik
tès ki pa-destriktif

API 5L GRB gaz ak lwil oliv liy tiyo faktori