Dyamèt deyò tiyo lwil oliv jeneralman varye ant 60.3 mm ak 114.3 mm.
Fòm yo pwosesis fen nan tiyo lwil oliv gen ladan: ki pa epè ak fil ak kouple, deyò epesè ak fil ak kouple, fen plenn, ki pa epesè ak fil ak kouple, deyò epesè ak fil ak kouple.
|
|
Trademark | Fòs rupture (MPa) | Fòs sede (MPa) | elongasyon (%) | dite |
|
API SPEC 5CT |
J55 |
Pi gran pase oswa egal a 517 |
379-552 |
0.5% |
- |
|
- |
K55 |
Pi gran pase oswa egal a 655 |
379~552 |
0.5% |
- |
|
- |
N80 |
Pi gran pase oswa egal a 689 |
552~758 |
0.5% |
- |
|
- |
L80(13Cr) |
Pi gran pase oswa egal a 655 |
552~655 |
0.5% |
Mwens pase oswa egal a 241HB |
|
- |
P110 |
Pi gran pase oswa egal a 862 |
758~965 |
0.6% |
- |
|
|
mak | konpozisyon chimik (%) |
- |
- |
- |
- |
- |
- |
- |
- |
- |
- |
|
C |
sizo |
Mn |
P |
S |
Kr |
Ni |
Taks |
Mo |
V |
Als |
- |
- |
|
API SPEC 5CT |
J55K55 (37Mn5) |
0.34-0.39 |
0.20-0.35 |
1.25-1.50 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.015 |
Mwens pase oswa egal a 0.15 |
Mwens pase oswa egal a 0.20 |
Mwens pase oswa egal a 0.20 |
Mwens pase oswa egal a 0.020 |
||
|
N80 (36 Mn2V) |
0.34-0.38 |
0.20-0.35 |
1.45-1.70 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.015 |
Mwens pase oswa egal a 0.15 |
- |
- |
- |
0.11-0.16 |
Mwens pase oswa egal a 0.020 |
- |
|
L80(13Cr) |
0.15-0.22 |
Mwens pase oswa egal a 1.00 |
0.25-1.00 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.010 |
12.0-14.0 |
Mwens pase oswa egal a 0.20 |
Mwens pase oswa egal a 0.20 |
- |
- |
Mwens pase oswa egal a 0.020 |
- |
|
P110 30CrMo) |
0.26-0.35 |
0.17-0.37 |
0.40-0.70 |
Mwens pase oswa egal a 0.020 |
Mwens pase oswa egal a 0.010 |
0.80-1.10 |
Mwens pase oswa egal a 0.20 |
Mwens pase oswa egal a 0.20 |
0.15-0.25 |
Mwens pase oswa egal a 0.08 |
Mwens pase oswa egal a 0.020 |
-
|