Tiyo asye san pwoblèm 34CrMo4 se yon tiyo asye alyaj ki gen gwo fòs ak segondè ki fabrike atravè yon pwosesis woule san pwoblèm.
Voye rechèch
Chat kounye a
Pwodwi Entwodiksyon

ekip tiyo gnee

Ki kalite tiyo asye san pwoblèm se klas 34CrMo4 la?
34CrMo4 se yon materyèl alyaj kwòm-molybdenum asye, ki se sitou itilize yo pwodwi materyèl tiyo asye san pwoblèm pou woule silenn gaz wo-presyon / silenn ak veso segondè-presyon.
Konpozisyon chimik materyèl 34CrMo4: C: 0.30~0.37 Si: Mwens pase oswa egal a 0.4{{10 }} Mn: 0.60~0.9{0 P, S: Mwens pase oswa egal a 0.020 P+S: Mwens pase oswa egal a 0.030 Cr: 0.90 ~ 1.20 Mo: 0.15 ~ 0.30 Ni: Mwens pase oswa egal a 0.30 Cu: Mwens pase oswa egal a 0.20
Estanda aplikasyon jeneral pou tiyo asye san pwoblèm pou silenn gaz 34CrMo4: estanda nasyonal GB/T 18248-2021, estanda Japonè JIS G 3429, estanda entènasyonal ISO 11120, estanda Ewopeyen an EN 10297-1, estanda Ameriken ASTM A372/A372M{ {8}}
Pwopriyete mekanik nan tib silenn gaz 34CrMo4: fòs rupture apre tretman chalè Pi gran pase oswa egal a 980Mpa, fòs sede Pi gran pase oswa egal a 835Mpa, elongasyon apre repo Pi gwo pase oswa egal a 12%, -50 degre enèji enpak tanperati ki ba. Pi gran pase oswa egal a 27J.
Tiyo asye 34CrMo4 yo jeneralman delivre nan yon eta woule oswa frèt-trase. Yo koupe ak trete nan silenn gaz oswa silenn asye ak Lè sa a, chalè trete ak tanperaman.

Konpozisyon chimik an % pa mas
Steel klas C sizo Mn P S Kr Mouvman Ni
34CrMo4 1.722 0,30 0,37 0,40 0,60 0,90 0,035 0,035 0,90 1,20 0,15 0,30
Pwopriyete mekanik pou tib ki fèt ak asye an akò ak kondisyon livrezon +QT
Steel klas Pwopriyete rupture minimòm
Non Steel Nimewo asye Fòs sede (ReH) Fòs rupture (Rm) A%
MPa MPa
Pou T nan mm Pou T nan mm Pou T nan mm
Mwens pase oswa egal a 8 > 8 > 20 > 50 Mwens pase oswa egal a 8 > 8 > 20 > 50 Mwens pase oswa egal a 8 > 8 > 20 > 50
Mwens pase oswa egal a 20 Mwens pase oswa egal a 50 Mwens pase oswa egal a 80 Mwens pase oswa egal a 20 Mwens pase oswa egal a 50 Mwens pase oswa egal a 80 Mwens pase oswa egal a 20 Mwens pase oswa egal a 50 Mwens pase oswa egal a 80
            l t l t l t l t
34CrMo4 1.722 800 650 550 500 1000 900 800 750 11 9 12 10 14 12 15 13

Tib asye san pwoblèm 34CrMo4

34CrMo4 Seamless Tubes For Gas Cylinders

 

Gwosè prensipal yo konvansyonèl nan tiyo asye san pwoblèm pou silenn gaz 34CrMo4 yo se: 108 * 4, 114 * 4, 139.7 * 4, 139.7 * 4.5, 139.7 * 5, 140 * 4, 140 * 4.5, 140 * 5, 203 * 5, 203. 203* 5.4, 229*5.3, ​​229*5.8, 232*5.3, ​​232*5.4, 267*5.7, 279*6.5, 279*6.8, 279*6, 316*7, 325*7.1*, 325*7.1*, 325*7.1* 16.8, 355.6 * 7.2, 355.6 * 7.4, 355.6 * 7.5, 356 * 7.2, 356 * 7.4, 356 * 7.5, lòt gwosè kapab tou Customized.

 

Anviwònman faktori Gnee

34CrMo4 Thin Wall Thickness Seamless Steel Pipe