ASTM A53/A106 san pwoblèm tiyo

Ki sa ki ASTM A106 ak ASTM A53?
ASTM A53 se spesifikasyon estanda pou tiyo, asye, nwa ak cho-tranpe, zenk-kouvwi, soude ak san pwoblèm. ASTM A106 se spesifikasyon estanda pou tiyo asye kabòn san pwoblèm pou sèvis wo-tanperati. API 5L se spesifikasyon pou liy tiyo.

Diferans ki pi enpòtan an se ke tiyo satisfè estanda A106 la dwe san pwoblèm pandan y ap rankontre tiyo A53 ka swa san pwoblèm oswa soude.

Konpozisyon chimik

Estanda Klas Konpozisyon chimik %
C Mn P S Si Kr Cu Ni Mo V
ASTM A106 B Mwens pase oswa egal a 0.30 0.29-1.06 Mwens pase oswa egal a 0.035 Mwens pase oswa egal a 0.035 >0.10 Mwens pase oswa egal a 0.40 Mwens pase oswa egal a 0.40 Mwens pase oswa egal a 0.40 Mwens pase oswa egal a 0.15 Mwens pase oswa egal a 0.08
ASTM A53 B Mwens pase oswa egal a 0.30 Mwens pase oswa egal a 1.20 Mwens pase oswa egal a 0.05 Mwens pase oswa egal a 0.045 Mwens pase oswa egal a 0.40 Mwens pase oswa egal a 0.40 Mwens pase oswa egal a 0.40 Mwens pase oswa egal a 0.15 Mwens pase oswa egal a 0.08

Tiyo asye kabòn ASTM A53 kouvri san pwoblèm, soude, nwa, ak cho-tranpe galvanised tiyo.

Estanda BS 1387, BS EN 10297, BS 4568, BS EN10217, JIS G3457
Klas 10#-45#, Cr-Mo alyaj, 15NiCuMoNb5, 10Cr9Mo1VNb, A53-A369
Soti dyamèt 21.3 - 610 mm
Epesè miray la 2 - 50 mm
Fòm Seksyon Wonn
Aplikasyon Tiyo likid
Tretman andigman vèni, bouchon, make
Sètifikasyon API
Kabòn Steel Tiyo ASTM A53/106/API 5L B
ST37/ST44 Precision tiyo asye san pwoblèm DIN 2448/2391/1629/17100
DIN 2391/2448/1629, ST37/ST52 tiyo asye ST37/ST52
Cho woule tiyo asye san pwoblèm ASTM A 53/106/API 5L B
Tib chodyè asye san pwoblèm trase frèt ASTM A106/DIN 17175/2448
Kabòn san pwoblèm tiyo asye ASTM A53/106/API 5L B

 