Pwopriyete chimik
Klas X60-PSL1 Liy tiyo lwil oliv ak gaz Konpozisyon chimik (%)
| Konpozisyon | C * | Mn* | P | S | Kr | Ni | Taks | Mouvman | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo san pwoblèm | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Maks | 0.28 | 1.4 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
| Konpozisyon | C * | Mn* | P | S | Kr | Ni | Cu | Mouvman | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo soude | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Maks | 0.26 | 1.4 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
Klas X60N-PSL2 Kabòn Steel liy tiyo konpozisyon chimik (%)
| Konpozisyon | C * | Si* | Mn* | P | S | Kr* | Ni* | Cu* | Mo* | Ti* | V * | Nb* | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | Min | - | - | - | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Maks | 0.24 | 0.45 | 1.4 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.04 | 0.1 | 0.05 | 0.001 |
Klas X60Q-PSL2 san pwoblèm liy asye tiyo konpozisyon chimik (%)
| Konpozisyon | C * | Si* | Mn* | P | S | Kr* | Ni* | Cu* | Mo* | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Max | 0.18 | 0.45 | 1.7 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
Tiyo klas X60M-PSL2 pou konpozisyon chimik likid ki ka pran dife (%)
| Konpozisyon | C * | Si* | Mn* | P | S | Kr* | Ni* | Cu* | Mo* | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo soude | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Maks | 0.12 | 0.45 | 1.6 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
Klas X65-PSL1 Tiyo liy san pwoblèm konpozisyon chimik (%)
| Konpozisyon | C * | Mn* | P | S | Kr | Ni | Taks | Mouvman | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo san pwoblèm | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Maks | 0.28 | 1.4 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
| Konpozisyon | C * | Mn* | P | S | Kr | Ni | Taks | Mouvman | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo soude | Min | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Maks | 0.26 | 1.45 | 0.03 | 0.03 | 0.5 | 0.5 | 0.5 | 0.15 | 0.001 |
Klas X65Q-PSL2 Kabòn Steel liy tiyo konpozisyon chimik (%)
| Konpozisyon | C * | Si* | Mn* | P | S | Kr* | Ni* | Cu* | Mo* | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Max | 0.18 | 0.45 | 1.7 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |
Klas X65M-PSL2 Kabòn Steel Tanperati segondè tiyo san pwoblèm konpozisyon chimik (%)
| Konpozisyon | C * | Si* | Mn* | P | S | Kr* | Ni* | Cu* | Mo* | B | Plis | |
|---|---|---|---|---|---|---|---|---|---|---|---|---|
| Tiyo soude | Min | - | - | - | - | - | - | - | - | - | - | Nb+V+Ti Mwens pase oswa egal a 0.15* |
| Maks | 0.18 | 0.45 | 1.6 | 0.025 | 0.015 | 0.5 | 0.5 | 0.5 | 0.5 | 0.001 |

Pwopriyete mekanik
Klas X60-PSL1 Tiyo pou transpò gaz gwo presyon Pwopriyete mekanik
| Kalite | Fòs rupture σb Mpa |
Pwen sede σs Mpa |
Elongasyon nan repo δ % |
|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | Pi gran pase oswa egal a 520 | Pi gran pase oswa egal a 415 | * |
Tiyo liy klas X60N-PSL2 pou lwil oliv ak gaz pwopriyete mekanik
| Kalite | Tanperati tès la | Fòs rupture σb Mpa |
Pwen sede σs Mpa |
Elongasyon nan repo δ % |
Enpak absòbe enèji KV2 J |
|---|---|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | 520~760 | 415~565 | * | ||
| OD mwens pase oswa egal a 20 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>20~30 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>30~36 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>36~48 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>48~56 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>56~84 | 0 degre | Pi gran pase oswa egal a 40 |
Klas X60Q-PSL2 Kabòn Steel liy tiyo pwopriyete mekanik
| Kalite | Tanperati tès la | Fòs rupture σb Mpa |
Pwen sede σs Mpa |
Elongasyon nan repo δ % |
Enpak absòbe enèji KV2 J |
|---|---|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | 520~760 | 415~565 | * | ||
| OD mwens pase oswa egal a 20 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>20~30 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>30~36 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>36~48 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>48~56 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>56~84 | 0 degre | Pi gran pase oswa egal a 40 |
Klas X60M-PSL2 lwil oliv ak gaz transmisyon tiyo Pwopriyete mekanik
| Kalite | Tanperati tès la | Fòs rupture σb Mpa |
Pwen sede σs Mpa |
Elongasyon nan repo δ % |
Enpak absòbe enèji KV2 J |
|---|---|---|---|---|---|
| Tiyo soude | 520~760 | 415~565 | * | ||
| OD mwens pase oswa egal a 20 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>20~30 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>30~36 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>36~48 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>48~56 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>56~84 | 0 degre | Pi gran pase oswa egal a 40 |

Klas X65-PSL1 Tiyo san pwoblèm pou gaz natirèl Pwopriyete mekanik
| Kalite | Fòs rupture σb Mpa |
Pwen sede σs Mpa |
Elongasyon nan repo δ % |
|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | Pi gran pase oswa egal a 535 | Pi gran pase oswa egal a 450 | * |
Klas X65Q-PSL2 Kabòn Steel liy tiyo pwopriyete mekanik
| Kalite | Tanperati tès la | Fòs rupture σb Mpa |
Pwen sede σs Mpa |
Elongasyon nan repo δ % |
Enpak absòbe enèji KV2 J |
|---|---|---|---|---|---|
| Tiyo san pwoblèm, tiyo soude | 535~760 | 450~600 | * | ||
| OD mwens pase oswa egal a 30 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>30~48 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>48~84 | 0 degre | Pi gran pase oswa egal a 54 |
Klas X65M-PSL2 Seamless Steel liy tiyo pwopriyete mekanik
| Kalite | Tanperati tès la | Fòs rupture σb Mpa |
Pwen sede σs Mpa |
Elongasyon nan repo δ % |
Enpak absòbe enèji KV2 J |
|---|---|---|---|---|---|
| Tiyo soude | 535~760 | 450~600 | * | ||
| OD mwens pase oswa egal a 30 | 0 degre | Pi gran pase oswa egal a 27 | |||
| OD>30~48 | 0 degre | Pi gran pase oswa egal a 40 | |||
| OD>48~84 | 0 degre | Pi gran pase oswa egal a 54 |
Aplikasyon:
Akòz fòs segondè ak rezistans presyon nan X65, li se souvan itilize nan lwil oliv ak gaz transpò tiyo anba pi wo presyon ak kondisyon tanperati, espesyalman nan aplikasyon pou kote pi long distans ak tèren pi konplèks yo mande nan sistèm transpò a.