Gwosè & pwa nan API 5dp fè egzèsis tiyo

Tiyo egzèsis‌ se materyèl debaz la manifaktire anba ‌API Spec 5d‌. 2023 revizyon estanda a prezante nouvo klas segondè - fòs asye ak ogmante pòs la - egzijans elongasyon frakti a ‌Pi gran pase oswa egal a 12%‌ (deja ‌Pi gran pase oswa egal a 10%‌).

Atravè kontwòl optimize nan fosfò ak kontni souf (‌P mwens pase oswa egal a 0.020%, s mwens pase oswa egal a 0.015%‌), sevè epesè miray tolerans (‌±10%‌), ak egzijans ranfòse dwat (‌Mwens pase oswa egal a 1.5 mm/m‌), estanda a asire amelyore ‌fòs torsyonèl‌ ak ‌rezistans korozyon‌ Pou tiyo egzèsis petwòl anba kondisyon konplèks jewolojik.

 

Spesifikasyon

Egalize: E-75, X-95, G-105, S-135

Aplikasyon: Pou byen perçage

 

Soti dyamèt tiyo egzèsis:

Soti nan 2 3/8 "a 6 5/8 ″

 

Longè chenn nan tiyo egzèsis:
Range 1: 18 pye a 22 pye.
Range 2: 27 pye a 30 pye.
Range 3: 38 pye a 45 pye.

 

Kalite tiyo egzèsis:
Tiyo egzèsis
Lou pwa egzèsis tiyo
Zouti jwenti
Pup jwenti

API 5CT drill pipe

Gwosè & pwa nan tiyo fè egzèsis:

Deziyasyon* Zouti done jwenti
Pipebody OD (pous) Poundage (liv pou chak pye) Egalize Fache kalite Rotary koneksyon zepòl OD (pous) PIN ID (pous) PIN OD longè* (pous) Box OD longè* (pous)
2-3/8 6.65 E Inuit NC26 3-3/8 1-3/4 7 8
2-3/8 6.65 X,G Inuit NC26 3-3/8 1-3/4 7 8
2-3/8 10.40 E Inuit NC31 4-1/8 2-1/8 7 9
2-3/8 10.40 X,G Inuit NC31 4-1/8 2 7 9
2-3/8 10.40 S Inuit NC31 4-3/8 1-5/8 7 9
3-1/2 9.50 E Inuit NC38 4-3/4 2-11/16 8 10-1/2
3-1/2 13.30 E Inuit NC38 4-3/4 2-11/16 8 10-1/2
3-1/2 13.30 X Inuit NC38 5 2-9/16 8 10-1/2
3-1/2 13.30 G Inuit NC38 5 2-7/16 8 10-1/2
3-1/2 13.30 S Inuit NC38 5 2-1/8 8 10-1/2
3-1/2 15.50 E Inuit NC38 4-3/4 2-9/16 8 10-1/2
3-1/2 15.50 X Inuit NC38 5 2-7/16 8 10-1/2
3-1/2 15.50 G Inuit NC38 5 2-1/8 8 10-1/2
3-1/2 15.50 S Inuit NC40 5-1/2 2-1/4 7 10
4 14.00 E Iu NC40 5-1/4 2-13/16 7 10
4 14.00 X Iu NC40 5-1/4 2-13/16 7 10
4 14.00 G Iu NC40 5-1/4 2-13/16 7 10
4 14.00 S Iu NC40 5-1/4 2-9/16 7 10
4 14.00 E Inuit NC46 6 3-1/4 7 10
4 14.00 X,G Inuit NC46 6 3-1/4 7 10
4 14.00 S Inuit NC46 6 3 7 10
4-1/2 16.60 E Inuit NC50 6-5/8 3-3/4 7 10
4-1/2 16.60 X Inuit NC50 6-3/8 3-3/4 7 10
4-1/2 16.60 G Inuit NC50 6-5/8 3-3/4 7 10
4-1/2 16.60 S Inuit NC50 6-3/8 3-1/2 7 10
4-1/2 20.00 E Inuit NC50 6-3/8 3-3/4 7 10
4-1/2 20.00 X Inuit NC50 6-5/8 3-1/2 7 10
4-1/2 20.00 G Inuit NC50 6-3/8 3-1/2 7 10
4-1/2 20.00 S Inuit NC50 6-5/8 3-1/4 7 10
4-1/2 16.60 E IEU NC46 6-1/4 3-1/4 7 10
4-1/2 16.60 X IEU NC46 6-1/4 3-1/4 7 10
4-1/2 16.60 G IEU NC46 6-1/4 3 7 10
4-1/2 16.60 S IEU NC46 6-1/4 2-3/4 7 10
4-1/2 20.00 E IEU NC46 6-1/4 3-1/4 7 10
4-1/2 20.00 X IEU NC46 6-1/4 3 7 10
4-1/2 20.00 G IEU NC46 6-1/4 2-3/4 7 10
4-1/2 20.00 S IEU NC46 6-3/8 2-1/2 7 10
5 19.50 E IEU NC50 6-5/8 3-3/4 7 10
5 19.50 X IEU NC50 6-5/8 3-1/2 7 10
5 19.50 G IEU NC50 6-5/8 3-1/4 7 10
5 19.50 S IEU NC50 6-5/8 2-3/4 7 10
5 19.50 E IEU 5-1/2fh 7 3-3/4 8 10
5 19.50 X,G IEU 5-1/2 FH 7 3-3/4 8 10
5 19.50 S IEU 5-1/2 FH 7-1/4 3-1/2 8 10
5 25.60 E NC50 6-5/8 3-1/2 3-3/4 7 10
5 25.60 X IEU NC50 6-5/8 3 7 10
5 25.60 G IEU NC50 6-5/8 2-3/4 7 10
5 25.60 E IEU 5-1/2 FH 7 3-1/2 8 10
5 25.60 X IEU 5-1/2 FH 7 3-1/2 8 10
5 25.60 G IEU 5-1/2 FH 7-1/4 3-1/2 8 10
5 25.60 S IEU 5-1/2 FH 7-1/4 3-1/4 8 10
5-1/2 21.90 E IEU 5-1/2 FH 7 4 8 10
5 21.90 X IEU 5-1/2 FH 7 3-3/4 8 10
5-1/2 21.90 G IEU 5-1/2 FH 7-1/4 3-1/2 8 10
5 21.90 S IEU 5-1/2 FH 7-1/2 3 8 10
5-1/2 24.70 E IEU 5-1/2 FH 7 4 8 10
5 24.70 X,G IEU 5-1/2 FH 7-1/4 3-1/2 8 10
5-1/2 24.70 S IEU 5-1/2 FH 7-1/2 3 8 10
6-5/8 25.20 E IEU 6-5/8 FH 8 5 8 11
6-5/8 25.20 X IEU 6-5/8 FH 8 5 8 11
6-5/8 25.20 G IEU 6-5/8 FH 8-1/4 4-3/4 8 11
6-5/8 25.20 S IEU 6-5/8 FH 8-1/2 4-1/4 8 11
6-5/8 27.70 E IEU 6-5/8 FH 8 5 8 11
6-5/8 27.70 X,G IEU 6-5/8 FH 8-1/4 4-3/4 8 11
6-5/8 27.70 S IEU 6-5/8 FH 8-1/2 4-1/4 8 11