Pwopriyete API 5L L450 liy tiyo

L450-PSL1 Konpozisyon chimik (%)

  konpozisyon Mn P S Kr Ni Cu Mo B Plis
Tiyo san pwoblèm Min - - - - - - - - - Nb+V+Ti Mwens pase oswa egal a 0.15
Max 0.28 1.4 0.03 0.03 0.5 0.5 0.5 0.15 0.001

 

  konpozisyon Mn P S Kr Ni Cu Mo B Plis
Tiyo soude Min - - - - - - - - - Nb+V+Ti Mwens pase oswa egal a 0.15
Max 0.26 1.45 0.03 0.03 0.5 0.5 0.5 0.15 0.001

 

L450-PSL1 Pwopriyete mekanik

Kalite Fòs rupture
σb
Mpa
Pwen sede
σs
Mpa
Elongasyon nan kraze oswa elongasyon
δ
%
San pwoblèm/soude Pi gran pase oswa egal a 535 Pi gran pase oswa egal a 450  
 

L450Q-PSL2 konpozisyon chimik (%)

  konpozisyon Si Mn P S Kr Ni Cu Mo B Plis
Tiyo san pwoblèm / soude Min - - - - - - - - - - Nb+V+Ti Mwens pase oswa egal a 0.15
Max 0.18 0.45 1.7 0.025 0.015 0.5 0.5 0.5 0.5 0.001

 

L450Q-PSL2 Pwopriyete mekanik

Kalite Tanperati tès la Fòs rupture
σb
Mpa

Pwen sede

σs
Mpa

Elongasyon nan kraze oswa elongasyon

δ
%

Enèji chòk absòbe
KV2
J

San pwoblèm/soude   535~760 450~600    
OD mwens pase oswa egal a 30 0 degre       Pi gran pase oswa egal a 27
OD>30~48 0 degre       Pi gran pase oswa egal a 40
OD>48~84 0 degre       Pi gran pase oswa egal a 54

 

L450M-PSL2 konpozisyon chimik (%)

  Konpozisyon Si Mn P S Kr Ni Cu Mo B Plis
Soude Min - - - - - - - - - - Nb+V+Ti Mwens pase oswa egal a 0.15
Max 0.18 0.45 1.6 0.025 0.015 0.5 0.5 0.5 0.5 0.001

 