API Spiral Weld Tiyo Tolerans

API espiral soude tiyo tolerans: Nan pwosesis pwodiksyon an, depi gwosè aktyèl la difisil pou reyalize egzijans gwosè nominal la, se sa ki, li souvan pi gwo oswa pi piti pase gwosè nominal la, estanda a presize ke yon diferans pèmèt ant gwosè aktyèl la. ak gwosè nominal la.

Atik

APISPE 5L

Mi tolerans epesè

D<508mm:A,B,A25+15%t-12.5%t

D>508mm:A,B,B25+17.5%t-12.5%t

X42-X80: +19.5% t-8.0%t

Kò tiyo

D<5{{1}8mm:±0.75%D

D{0}}-914mm:±0.75%D-0.25%D

D>914mm: +6.35-3.2mm

Tiyo fen longè ranje

D<273.1mm: +1.59mm-0.4mm

D=323.9-�% bc�508mm{{3}.38mm

D>5{{1}8%-0.79mm

Tiyo fen ovalite

D<508mm:-

D>508mm:±1%D

Weld ranfòsman

t Mwens pase oswa egal a 12.7mm: Mwens pase oswa egal a 3.18mm

t>12.7mm: Mwens pase oswa egal a 4.76mm

Tiyo fen oswa bizote laminasyon sifas oswa enklizyon salop

transverse Mwens pase oswa egal a 6.35mm

 

Spesifikasyon Valè
Estanda tiyo API 5L
Kalite tiyo Tiyo soude espiral
Materyèl Kabòn Steel, Low Alloy Steel
Ranje gwosè tiyo OD: 219 mm - 3620 mm
Epesè miray la Varye selon kondisyon OD ak presyon
Longè Varye (yon sèl o aza, doub o aza, longè fiks)
Kouch 3LPE, FBE, penti nwa, elatriye.
Aplikasyon Lwil oliv ak gaz, transmisyon dlo, objektif estriktirèl
Avantaj Segondè fòs, bon rezistans nan korozyon, pri-efikas pou gwo dyamèt
Tès Tès idrostatik, Tès ki pa destriktif (NDT)
Pwosesis Faktori Soude Arc Submerged Spiral (SSAW)

API Spiral Weld Pipe