Ki klas ASTM A106 tiyo?

A106 se sèlman pwodwi kòm yon pwodwi san pwoblèm epi li disponib nan twa klas; A, B, C. Pa gen kalite nan A106 paske li pwodui sèlman kòm yon pwodwi san pwoblèm. A53 vini nan de klas ak twa kalite.

 

Tablo konpozisyon chimik:

Estanda Klas Pwosesis Konpozisyon chimik %
C max Mn* P max S max Si min Kr˟ max Kou max Ni% cb� max Mo% cb� max V˟ max
ASTM A106-15 B kontinan yo 0.30* 0.29-1.06 0.035 0.035 0.10 0.40 0.40 0.40 0.15 0.08
ASTM A106-15 C kontinan yo 0.35* 0.29-1.06 0.035 0.035 0.10 0.40 0.40 0.40 0.15 0.08
ASTM A53-12 B kontinan yo 0.30* 1.20 0.05 0.045 --- 0.40 0.40 0.40 0.15 0.08

Tablo Pwopriyete Mekanik:

Estanda Klas    
Pwosesis Fòs rupture (MPa) Min Fòs Sede (MPa) Min Elongasyon nan 2" (%) MinimumLong. Tès dezabiye Elongasyon nan 2" (%) MinimumTrans. Tès Strip
ASTM A106-15 B kontinan yo 60,000 [415] 35,000 [240] 30 16.5
ASTM A106-15 C kontinan yo 70,000 [485] 40,000 [275] 30 16.5
ASTM A53-12 B kontinan yo 60,000 [415] 35,000 [240] 30 Gade Spec